Language: ChineselineEnglish

News

Why is ozone decomposition catalyst prone to deactivation in high‑humidity environments?

In high‑humidity environments, the activity of manganese‑based, copper‑manganese mixed oxide, and Hopcalite‑type ozone decomposition catalysts can decline significantly or even be completely lost. This deactivation is not caused by a single factor, but rather results from three mechanisms working together: competitive adsorption between water molecules and ozone for active sites on the catalyst surface, chemical passivation of active sites due to surface hydroxylation from water dissociation, and irreversible structural degradation and by‑product accumulation induced by long‑term exposure to water. Understanding these three mechanisms is the theoretical prerequisite for analyzing the problem of ozone catalytic decomposition under high‑humidity conditions. Each is discussed below.

Ozone O3 Destruct Treatment Catalyst

I. Competitive adsorption: water molecules preferentially occupy active sites

The first step in ozone decomposition catalysis is the adsorption of ozone molecules onto the active centers of the catalyst surface. For transition metal oxide catalysts, these active centers are typically unsaturated coordination metal ions or oxygen vacancies, which possess unpaired electrons or dangling bonds and can form chemisorption bonds with ozone.

Water molecules have a very strong polarity, much stronger than that of ozone. More importantly, water molecules can coordinate with metal ions through the lone pair electrons on the oxygen atom, and their adsorption energy is generally significantly higher than that of ozone. Under dry conditions, ozone can successfully occupy these sites and undergo subsequent reactions; once water vapor is present in the environment, water molecules preferentially adsorb and occupy the sites for a long time, forming a physical adsorption layer or water film on the catalyst surface.

The direct consequence of competitive adsorption is that ozone molecules have difficulty reaching the active interface, and macroscopically the catalyst shows a marked decrease in apparent reaction rate. This effect is even more pronounced at lower temperatures because capillary condensation is more likely to occur, further exacerbating site blockage. In addition, the hydrogen‑bonding network formed by water molecules on the surface also limits the surface diffusion ability of ozone molecules – even if a small amount of ozone successfully adsorbs, it cannot readily migrate to adjacent sites to complete the decomposition reaction. This physical competition mechanism is the most direct and fastest‑responding way in which humidity affects the catalyst, and its impact is positively correlated with the relative humidity of the environment.

II. Surface hydroxylation: chemical passivation of active sites

Competitive adsorption is mainly a physically reversible process – some activity can be restored after drying. However, water molecules do not only physisorb on the catalyst surface; they also undergo dissociative chemisorption to form surface hydroxyl groups (–OH), which is a chemical change process.

Taking manganese oxide as an example, water molecules can dissociate at metal ion bridges near surface oxygen vacancies, forming two adjacent surface hydroxyl groups. The formation of surface hydroxyl groups brings three key consequences.

First, hydroxyl groups block the electron‑transfer channels necessary for ozone decomposition. The ozone decomposition process requires metal ions to cycle between different valence states (e.g., Mn⁴⁺/Mn³⁺ or Cu²⁺/Cu⁺). After hydroxyl groups coordinate with metal ions, the coordination of the metal ions tends to become saturated, and their redox reversibility is suppressed, making it difficult for electrons to transfer between the catalyst surface and ozone molecules.

Second, surface hydroxyl groups change the adsorption mode of ozone on the catalyst surface. On a clean oxide surface, ozone normally undergoes chemisorption to form stable adsorbed intermediate species; on a surface with high hydroxyl coverage, ozone can only undergo weak physisorption and has difficulty proceeding further to the decomposition reaction. In situ spectroscopic studies can confirm that under high‑humidity atmospheres, typical reaction intermediates are not detected on the catalyst surface; instead, characteristic signals of adsorbed water and hydroxyl groups appear.

Third, the hydrogen‑bonding network formed between hydroxyl groups and between hydroxyl groups and surface oxygen hinders the surface migration of key reactive oxygen species generated during ozone decomposition. The reactive oxygen atoms produced by ozone decomposition need to move on the surface and meet to combine into oxygen molecules. The hydroxyl network divides the surface into many isolated hydrated micro‑domains, trapping reactive oxygen in local regions so that they cannot easily undergo dimerization, causing the reaction to stall at an intermediate step. This mechanism explains why even after water is removed, catalyst activity is difficult to fully recover – removal of surface hydroxyl groups requires higher energy (typically heating to 200‑300°C or above), which cannot be achieved by ordinary room‑temperature drying.

III. Water‑induced structural degradation and by‑product accumulation

If the first two mechanisms are reversible to some extent, the third – irreversible structural changes and by‑product accumulation induced by long‑term water exposure – is the root cause of eventual catalyst报废 (failure).

Structural degradation mainly manifests in the following aspects. First, many ozone decomposition catalysts (especially amorphous or nanocrystalline transition metal oxides prepared by coprecipitation) undergo hydration in water or high‑humidity atmospheres, leading to lattice expansion and phase transformation. For example, certain layered manganese oxides can gradually transform into hydrated layered mineral phases in humid atmospheres; during this process, a large number of active edge sites are lost and the specific surface area decreases significantly. Second, repeated water adsorption‑desorption cycles cause grain growth, degrading the nanoscale active structure into micron‑sized crystals and losing the high specific surface area characteristic. Third, for shaped catalysts (e.g., honeycomb, spherical, or granular), repeated water adsorption and desorption cause volume expansion and contraction, generating microcracks that eventually lead to catalyst pulverization, increased bed pressure drop, and even loss of active components. In addition, for catalyst formulations containing soluble promoters (e.g., certain alkali metal ions), once a water film forms, these promoters may dissolve and migrate with condensed water, leading to uneven distribution or even complete loss of the promoters, thereby destroying the electron‑modulating function of the catalyst.

By‑product accumulation is also not negligible. In the presence of water, the decomposition pathway of ozone may change. Ozone can react with surface hydroxyl groups or adsorbed water to generate hydrogen peroxide; hydrogen peroxide may further decompose on the transition metal surface, but some of it may form stable peroxo complexes with metal ions, covering the active sites. Furthermore, carbon dioxide from the air dissolves into the water film to form carbonic acid, which then reacts with surface metal ions to form carbonate precipitates. The thermal decomposition temperature of carbonates is usually much higher than the conventional regeneration temperature of catalysts, so once formed, they can be considered permanent poisons. These by‑products accumulate on the catalyst surface, further blocking pores and covering active sites, leading to irreversible deactivation.

In summary, the impact of high‑humidity environments on ozone decomposition catalysts is systemic, multi‑level, and partially irreversible. Physical competitive adsorption causes acute deactivation, surface hydroxylation causes sub‑acute passivation, and structural degradation together with by‑product accumulation determines the ultimate service life of the catalyst. In actual working conditions, these three mechanisms often occur simultaneously and exacerbate each other, making high humidity one of the most challenging operating environments for ozone decomposition catalysts.


author:Gloria
date:2026-05-19


CATEGORIES

    CONTACT US

    Contact: Candyly

    Phone: +8618142685208

    Tel: 0086-0731-84115166

    Email: sales@minstrong.com

    Add: E2 Building, Kinglory Science And Technology Industrial Park, Wangcheng Area, Changsha, Hunan, China.