In ozone abatement for semiconductor wafer fabrication, the core selection decision is not which catalyst has the highest initial efficiency number, but whether it can maintain stable compliance under the target space velocity and actual humidity conditions. Cleanrooms in wafer fabs face a combined operating condition of ppm-level ozone concentrations and process airflows of tens of thousands of m³/h, where the reaction driving force is limited and contact time is compressed. The superposition of these two factors makes the effective utilization of catalyst active sites the decisive variable. Around this judgment, catalyst selection requires a complete logical chain from operating condition characterization, core contradiction decomposition, key engineering dimension assessment, to loading calculation. A mismatch in any one dimension may manifest as efficiency decay or shortened service life after several months of operation.

The use of ozone in semiconductor manufacturing spans multiple process steps. Ozone water cleaning utilizes the strong oxidizing power of ozone to remove photoresist residues and organic contaminants from wafer surfaces. Ozone water concentrations typically range from 2–20 ppm, and some processes can reach 50–100 ppm. Dissolved ozone continuously escapes during circulation and drainage, with relatively concentrated levels near cleaning tank openings and drain ports. UV ozone cleaning is another major source: 185 nm short-wavelength UV light photolyzes oxygen in air to generate ozone. A study measured the working environment of a hard disk component factory using short-wavelength UV technology and found ozone concentrations around the equipment exceeding 150 ppb. In addition, corona discharge equipment, plasma processing equipment, and static eliminators at the top of cleanrooms continuously generate ozone during operation. Fresh air introduced by HVAC systems also deserves attention. When ambient ozone concentrations rise in summer, HEPA/ULPA filters have almost no retention capacity for ozone molecules, allowing outdoor ozone to enter the clean environment.
These escaping ozone emissions create a continuous low-concentration load in the cleanroom, and the enclosed nature of the cleanroom makes natural dissipation contribution extremely limited. The natural decomposition half-life of ozone is about 50 minutes, but cleanroom air exchange rates are limited, so natural decomposition alone cannot maintain compliance. Control standards are quite strict: GBZ 2.1-2019 specifies a maximum allowable concentration of 0.3 mg/m³ for ozone in workplace air; OSHA sets an 8-hour time-weighted average permissible exposure limit of 0.1 ppm (about 0.2 mg/m³); and NIOSH recommends a ceiling limit of 0.1 ppm. In practice, semiconductor cleanrooms typically use below 0.1 ppm as a safety reference standard.
It is particularly worth noting that ppb-level ozone poses a non-negligible risk to the process itself. Photolithography is most sensitive to ozone. After ozone reacts with organic components on the photoresist surface, it alters their chemical structure, manifesting as linewidth control failure, pattern edge roughness, and other defects. Exposed metal interconnect layers accelerate oxidation in an ozone environment. Copper, silver, and aluminum surfaces form oxides or corrosion products, which not only increase contact resistance but may also lead to metal line breakage or bridging shorts. Polymer seals, tubing, and cable sheaths widely used in cleanrooms accelerate aging under long-term low-concentration ozone exposure. Once released submicron particles settle on wafer surfaces, they form killer defects. Among the three mainstream technical paths—activated carbon adsorption, thermal decomposition, and catalytic decomposition—catalytic decomposition, with its room-temperature operation and no secondary pollution, has become the applicable solution for low-concentration, high-airflow scenarios.
The resulting operating condition profile has several constraining characteristics: ozone concentrations in the ppm to tens of ppm range, process airflows typically in the thousands to tens of thousands of m³/h, ambient temperature around 25°C, relative humidity of 40%–60%, and over 80% in wet process areas. Among these, high space velocity is the constraint that must be faced squarely.
Space velocity (GHSV) represents the volume of gas treated per unit volume of catalyst per hour. The higher the space velocity, the smaller the equipment volume and the greater the treatment capacity, but the shorter the residence time of gas in the catalyst bed. Ozone decomposition requires effective contact between ozone molecules and active sites on the catalyst surface. Insufficient contact time means some ozone molecules pass through the bed without completing the reaction. Studies have shown that at a space velocity of 120,000 h⁻¹, the ozone removal rate drops to 78.6% after the catalyst treats about 1 g of ozone, while at 60,000 h⁻¹, the removal rate remains at a relatively high level after treating 1.25 g of ozone. The design space velocity for semiconductor cleanrooms typically needs to be controlled between 10,000 and 50,000 h⁻¹, lower than design values for conventional industrial waste gas treatment. The upper limit of this range is constrained by contact time, while the lower limit is constrained by equipment volume and the engineering feasibility of pressure drop.
Under low-concentration conditions, the number of ozone molecules reaching active sites per unit time is inherently limited, and excessively high space velocity further compresses the effective reaction amount. The engineering consequence of this contradiction is reflected in the logic of selection judgment: the 99% efficiency measured in the laboratory under low space velocity and dry gas conditions often cannot be reproduced under the actual space velocity and humidity conditions of a cleanroom. For semiconductor production lines, catalyst replacement means downtime maintenance, and maintenance costs inside a cleanroom are far higher than the catalyst itself. Therefore, the indicator that truly matters is how long efficiency can be maintained under the target space velocity and actual humidity conditions.
Manganese-based composite oxides have good applicability in room-temperature, low-concentration ozone decomposition scenarios, and their catalytic activity is closely related to surface Mn³⁺ content and oxygen vacancy concentration. According to published research reports, the surface Mn³⁺ content of manganese oxides can be regulated by controlling hydrothermal parameters, and this content is positively correlated with catalytic activity. Other studies have constructed manganese oxide systems rich in surface hydroxyl groups, maintaining 100% ozone conversion within 240 minutes at relative humidity not exceeding 50%, and still maintaining 90% conversion within 240 minutes at 90% relative humidity. The ozone decomposition performance of non-precious metal manganese-based catalysts at room temperature has been verified by many studies, and their cost structure makes them applicable in industrial scenarios. It should be noted that semiconductor scenarios have higher requirements for material purity than general industrial scenarios. The leaching of metal ions from catalysts and supports may cause irreversible contamination to wafers, so stricter entry thresholds must be set for active phase selection and support purity control.
The design space velocity for ozone abatement in semiconductor cleanrooms typically needs to be controlled between 10,000 and 50,000 h⁻¹. For scenarios with low ozone concentration but large airflow, choosing a lower space velocity means a larger catalyst volume and higher equipment investment, but it can trade for longer contact time and more stable efficiency output. During selection, a balance must be found between equipment investment and operational stability, rather than blindly pursuing high space velocity to reduce equipment volume.
Honeycomb catalysts have regular gas flow channels and low fluid resistance, and their pressure drop is significantly lower than that of granular beds under the same space velocity. At a space velocity of 20,000 h⁻¹, the pressure drop of a monolithic honeycomb catalyst bed is typically below 200 Pa, while a granular bed can reach 800–1,500 Pa, only one-fifth to one-tenth of the latter. The geometric specific surface area of honeycomb catalysts can reach 1.5–3.0 m²/g. The parallel channel structure causes gas to pass through in a laminar or transitional flow state, with a thinner boundary layer, which facilitates convective mass transfer of ozone molecules to the channel walls. In laboratory tests, monolithic catalysts can stably achieve over 95% decomposition efficiency for 30 ppm ozone (25°C, 40% relative humidity). In addition, honeycomb structures have a lower wear tendency than granular beds, reducing the risk of particulate release, which is an important safety redundancy in clean environments of ISO Class 3 or higher. Granular catalysts still have anti-clogging advantages in pretreatment sections with higher dust content, but in the terminal purification stage of semiconductor cleanrooms, honeycomb structures are usually the more reasonable choice.
Cleanrooms are typically maintained at 40%–60% relative humidity, but wet process areas and rainy seasons in southern factories can push relative humidity above 80%. Water molecules and ozone undergo competitive adsorption on catalyst active sites. Under high humidity, the decomposition efficiency of ordinary manganese-based catalysts can drop from 98% to below 70% within 24 hours. In recent years, significant progress has been made in moisture-resistant modification research. Some studies have applied an external electric field to the surface of manganese oxides via an electrochemical strategy to suppress competitive adsorption of water molecules, maintaining ozone conversion above 94% during 48 hours of continuous operation at 90% relative humidity. Other studies have used potassium-ion-doped layered manganese dioxide structures, which exhibit good ozone decomposition performance under both low-temperature and high-humidity conditions, with no observed accumulation of peroxide intermediates on the surface. The poisoning risk of sulfur compounds to catalysts also needs to be assessed. According to published research, the main reason for the deactivation of Mn-based catalysts in SO₂-containing atmospheres is that SO₂ is oxidized to sulfate species with the assistance of O₃, occupying oxygen vacancies and hindering electron transfer between Mn and O, leading to decreased low-temperature reducibility and oxygen vacancy concentration. During selection, it is necessary to distinguish between "dry gas condition efficiency" and "steady-state efficiency under actual humidity conditions," and require suppliers to provide performance data within the target humidity range.
Loading calculation starts with the space velocity formula: catalyst volume equals process airflow divided by design space velocity. For a cleanroom ozone abatement system with a process airflow of 10,000 Nm³/h, if the design space velocity is 15,000 h⁻¹, the required catalyst volume is approximately 0.67 m³. However, in engineering practice, a safety margin must be added on top of the design space velocity, considering factors such as activity decay caused by humidity fluctuations, efficiency decline of the catalyst over its service life, and short-term fluctuations in ozone concentration. For semiconductor scenarios, the safety margin should be set more conservatively than for conventional industrial scenarios.
HG/T 5419-2018 "Test Method for Activity of Manganese-Based Ozone Decomposition Catalysts" has been in effect since April 1, 2019. It applies to catalysts with manganese dioxide as the main active component for decomposing ozone in the environment and provides a unified evaluation framework for performance comparison among different suppliers. However, the activity data given by this standard are obtained under standard test conditions, and procurement decisions still need to be judged in combination with specific operating parameters.
Regarding data verification, a practical approach is to require suppliers to provide actual operating data as close as possible to the target operating conditions—space velocity range, humidity range, and ozone concentration range. Operating cases in similar semiconductor cleanrooms or electronics manufacturing clean workshops have higher reference value than test reports under ideal conditions. In addition, attention should be paid to the efficiency decay curve of the catalyst over its service life, rather than only initial efficiency data, because the compliance requirements of semiconductor production lines for emission concentrations are continuous. The modular design of monolithic catalysts can reduce replacement downtime from 2–3 days for traditional granular beds to 4–8 hours. This engineering characteristic is also worth considering when evaluating life-cycle costs.
Take a local exhaust ventilation purification project in an electronics manufacturing clean workshop as an example (without naming specific companies). The ozone in this workshop mainly comes from UV cleaning equipment. The exhaust airflow is 8,000 m³/h, the inlet ozone concentration is about 5 ppm, the ambient temperature is 24°C, and the relative humidity is 55%. The design space velocity is 12,000 h⁻¹, and the loading amount of honeycomb manganese-based catalyst is approximately 0.67 m³. After 6 months of operation, the outlet ozone concentration remained below 0.05 ppm, and the catalyst bed pressure drop showed no significant increase. This case indicates that, under the premise of reasonable selection of space velocity and support geometry, manganese-based catalysts can achieve relatively long-term stable operation in semiconductor-related clean environments. It should be noted that the operating data of this case come from actual engineering monitoring, and the specific decay rate still needs to be tracked for more than 12 months for confirmation.
Under low-concentration, high-space-velocity conditions, the criterion for judging catalyst suitability is not "the highest efficiency number," but whether it can maintain stable compliance within its design life under the target space velocity and actual humidity conditions. This requires systematic evaluation across several dimensions: selection of the active phase system, matching of space velocity and catalyst volume, influence of support geometry on pressure drop and cleanliness, and moisture resistance and poisoning resistance. A mismatch in any one dimension may manifest as efficiency decay or shortened service life after several months of operation. For semiconductor wafer fabrication, an application scenario with extremely high requirements for cleanliness, stability, and continuity, the engineering logic of selection should take priority over parameter comparison.
Contact: Candyly
Phone: +8618142685208
Tel: 0086-0731-84115166
Email: sales@minstrong.com
Add: E2 Building, Kinglory Science And Technology Industrial Park, Wangcheng Area, Changsha, Hunan, China.